Is there any risk of galvanic corrosion risk with BPTA-DTMC Touchaqua Digit Thermal Sensor
asked
Nov 23, 2019
in
Product related
by
anonymous
I'm using copper radiators with nickle/plexi water-blocks and nickle fittings. I'd like to know what material is used in the following item and if there is any risk of galvanic corrosion:
Bitspower Touchaqua Digit Thermal Sensor
Brand:
Bitspower Touchaqua
Product Code: BPTA-DTMC
UPC: 885488001240
EAN: 4711946731243
bpta-dtmc
thermal-sensor
compatibility
water-cooled
Please
log in
or
register
to answer this question.
1
Answer
answered
Nov 26, 2019
by
lily
(
123k
points)
Hello, the main material of BPTA-DTMC is POM. So there no risk of galvanic corrosion.