I'm using copper radiators with nickle/plexi water-blocks and nickle fittings. I'd like to know what material is used in the following item and if there is any risk of galvanic corrosion:

Bitspower Touchaqua Digit Thermal Sensor

1 Answer

answered by (123k points)
Hello, the main material of BPTA-DTMC is POM. So there no risk of galvanic corrosion.

Any questions, feel free to contact us.

 

 

 

 

 

...